High Strength, Heat Treated Alloys - Comparison Chart (Kromite#3 /
Mirraloy TGP / SAE 4000 Series)

Mirraloy TG&P and Kromite #3

SAE 4000 Series

ELECTRIC FURNACE MELT
• smaller more refined chemistry
• more control of heat lot

OPEN HEARTH FURNACE
• large heats - less refinement
• little control

CLEAN STEEL TECHNOLOGY
• manufacturing process to eliminate
impurities in steel and improve fatigue
resistance

NOT REQUIRED
VACUUM DEGASSING
• removes impurities in the steel to refine the
chemistry

NOT REQUIRED

UNIQUE CHEMISTRY
• low phosphorus, low sulfur, nickel
enhanced
• cleaner chemistry and improved strength

STANDARD CHEMISTRY
• commercial practice follows minimum
standards

HEAT TREATED
• thermal process is verified against strict
guidelines

HEAT TREATED
• lacks depth and uniformity compared to
Kromite #3 and Mirraloy TG&P

PHYSICAL PROPERTIES
• typical tensile strength 156K
• typical yield strength 123K
• typical hardness Rockwell "C" 30/32

PHYSICAL PROPERTIES
• typically 20% less strength than Kromite #3
and Mirraloy TG&P
• more susceptible to fatigue failure

MACHINE STRAIGHTENED
• one half of the industry standard; 1/8" in any 5 feet

MACHINED STRAIGHTENED
• 1/4" in any 5 feet

STRESS RELIEVED
• thermal treatment process to reduce the
chances of "walking" or movement during
machining
NOT REQUIRED
FATIGUE RESISTANCE
• excellent toughness
• toughness resists fatigue failure
FATIGUE RESISTANCE
• lower degree of toughness - subject to
fatigue failure, the number one cause of
shaft failure in heavy industry
MACHINABILITY
• fine uniform grain promotes ease of
machining
MACHINABILITY
• not consistent, hard and soft spots
MECHANICAL TESTING
• Tensile, yield, elongation, reduction of area,
and jominy are checked every 10,000 lbs,
resulting in better control over physicals

MECHANICAL TESTING
• commercially done at 50,000 lbs increments
• less control of physical properties
Designed to provide optimum performance.
SAE establishes safe minimum standards,

Designed to provide optimum performance. SAE establishes safe minimum standards,
not intended to provide optimum
performance.

View our online catalog for PDF brochures on these and other products.

 
 
Home  |  Products  |  News Updates  |  Terms of Sale  |  ISO Certificate  |  Links  |  Contact Us
© Assocated Steel Corporation    E-mail: mail@associatedsteel.com    Powered by Dynamics Online, Inc.